#1
|
|||||
|
|||||
![]()
__________________
Doug |
#3
|
|||||
|
|||||
![]() I don't think I've used the Vertex stuff. It was old D-D epoxy I was using. The P-off is that it didn't even harden, and I ended up re-doing some pieces with some fresh TLF epoxy. I find neither the D-D nor the TLF are easy to work with - they don't stick well. I used to love the Boston Aqua Farms epoxy, but the LFS doesn't carry it anymore.
|
#4
|
|||||
|
|||||
![]() Did you do it in the microwave first?
__________________
Reef Pilot's Undersea Oasis: http://www.canreef.com/vbulletin/sho...d.php?t=102101 Frags FS: http://www.canreef.com/vbulletin/sho...d.php?t=115022 Solutions are easy. The real difficulty lies in discovering the problem. |
#6
|
|||||
|
|||||
![]() Yes I did.
I did that on a few that were particularly troublesome, but it didn't help. The glue wouldn't stick to the epoxy. ![]() |
#7
|
|||||
|
|||||
![]() Well, very sorry to hear your troubles. You had some nice frags there. Hope the rest survive OK.
__________________
Reef Pilot's Undersea Oasis: http://www.canreef.com/vbulletin/sho...d.php?t=102101 Frags FS: http://www.canreef.com/vbulletin/sho...d.php?t=115022 Solutions are easy. The real difficulty lies in discovering the problem. |