#1
|
||||
|
||||
![]() I'm going to practice by trying to build something similar on a much smaller scale, I need a skimmer fro my nano with no sump. I don't see why a recirc can't work for that as well, with a small feed pump immersed in the tank proper and outflow going directly back in the tank from the skimmer placed slightly higher than the tank itself on an adjacent shelf or cabinet. Does that sound like something that would work?
|
#2
|
|||||
|
|||||
![]() Look for a GE plastics or SABIC (new name) listing in NL; typically your best source for weld-on and acrylic.
__________________
By reading, replying to, commenting about, or in any way accessing the material in this post; including but not limited to storing in a database, retrieving from a database, viewing in a web browser, including it in or making a reference to it in a legal document, or accidentally glancing at it you agree to send me $100. |
#3
|
||||
|
||||
![]() Apparently there is a location in Halifax,
http://www.sabicpolymershapes.com/po...ernational.jsp |
#4
|
|||||
|
|||||
![]() Just curious. Where are you getting the acrylic for this project? They should certainly have solvent....
__________________
Brad |
#5
|
||||
|
||||
![]() Yes, they do but they're charging $42 for a can of weldon #3! And they don't have either of #16 or #40, which I'd prefer given this is my first such project.
|
#6
|
|||||
|
|||||
![]() You want to use 3. 16 is just sloppy and 40 is a 2 part mix that it a hassle to work with. A bit of practice and #2 or 3 will be fine.
A small can of 3 should be a couple of bucks.
__________________
Brad |
#7
|
||||
|
||||